Instrument information  

Brand: TA Instrument

Model: DSC Q200

Temperature Range: -90oC to 400oC

Principle: The Differential Scanning Calorimeter (DSC) instruments determine the temperature and heat flow associated with material transitions as a function of time and temperature. They provide quantitative and qualitative data on endothermic (heat absorption) and exothermic (heat evolution) processes of materials during physical transitions such as phase changes, melting, oxidation, and decomposition. This information helps the scientist or engineer identify processing and end-use performance.

Sample Types: 

  1. Film
  2. Powder
  3. Liquid

Sample Weight: 5 to 20 milligrams

Instrument Status: Good

Location: Level 1, Structure and Thermal Laboratory, Block B, Department of Physics.



To submit a test request, click here to access the online request form.

For the latest testing prices, click here.

Last Update: 23/10/2026